Firing guide
Every Sarbokh clay fires to the same range, which means you can fire pieces made from different bodies in one kiln load.
10001300
- Biscuit firing
- 1075°C
- Glaze firing
- 1180–1220°C
Biscuit firing
1075°C
The first firing of the dried piece. It sets the form and makes it ready to glaze.
Glaze firing
1180–1220°C
The second firing after glazing, where the piece becomes hard, sealed stoneware.
Products and their firing range
| Product | Biscuit firing | Glaze firing |
|---|---|---|
| Underglaze Colours 300 ml | — | 1180–1220°C |
| Underglaze Colours 60 ml | — | 1180–1220°C |
| White Casting Slip | 1075°C | 1180–1220°C |
| Yellow Ceramic Clay | 1075°C | 1180–1220°C |
| Black Ceramic Clay | 1075°C | 1180–1220°C |
| Pearl White Ceramic Clay | 1075°C | 1180–1220°C |
| White Ceramic Clay | 1075°C | 1180–1220°C |